Different repair routes for support rollers, tyres and shafts
The support-roller hardfacing proposal starts with cleaning and inspection, roughening and cleaning, and defect removal to sound substrate. Preheating, layered FGM-KM-B.U deposition, stress relief, rough grinding and finish grinding follow, then inspection and handover. Dye penetrant testing checks defect removal; delivery checks cover appearance, dimensions, hardness and ultrasonic testing of the repair area. The off-line plan also specifies a bogie-hearth electric annealing furnace: treat the rebuilt part to the temperature curve, cool slowly to relieve stress, then turn and grind to drawing dimensions.
Tyre repair welding uses φ1.2 flux-cored and φ1.2 solid wire, with KM1# for the bonding layer and KM3# for the working layer. Equipment comprises an NB500 gas-shielded welder and a 500A wire feeder. A radius template made to the tyre dimensions, together with a steel rule and feeler gauges, checks the repaired surface. A Henan cement-enterprise plan requires the repaired surface to differ from adjacent undamaged areas by ≤0.5 mm, measured with the rule and feeler gauges, with surface finish ≤Ra3.2 and satisfactory flaw detection before handover.
Worn main-shaft areas are restored with FGM-KM-B.U before precision machining on an on-line external lathe. A bearing-seat enquiry must distinguish the journal outside diameter from the bearing-housing bore. The outside diameter combines material restoration and external machining; the bore combines on-line bore repair and on-site boring. Roll working surfaces use a dedicated submerged-arc hardfacing machine, followed by on-site machining of roll-shaft mating sections.
Robotic laser cladding provides an additional route for shafts, rolls, gears and valves, off-line in the workshop or on-line. The cross-shaft plan first records shaft-location roundness, straightness and end-face condition, then preheats to 300℃ and aligns the part on a horizontal lathe. Layered robotic cladding is monitored for pores, inclusions and cracks. Stress relief at 300℃ and furnace cooling precede precision turning. Final checks cover HRC58-60, shaft-location and end-face dimensions, coaxiality, straightness and roundness. Each operation must pass reinspection before the next.
Those temperature and hardness values belong to the cross-shaft plan. Other components require values based on their substrate, original heat treatment and drawing.