First establish the location and extent of the abnormality in accordance with the inspection requirements for this kiln tyre, then determine the corrective plan. The records on the official website specify ultrasonic testing before and after kiln tyre crack repair, whereas dye penetrant testing in the shell repair plan verifies defect removal. The components and inspection stages are different.
First establish the location and extent of the abnormality in accordance with the inspection requirements for this kiln tyre, then determine the corrective plan. The records on the official website specify ultrasonic testing before and after kiln tyre crack repair, whereas dye penetrant testing in the shell repair plan verifies defect removal. The components and inspection stages are different.
First Identify Whether the Inspection Concerns a Kiln Tyre or the Surface Exposed by Defect Removal on a Shell
The crack repair information on the official website of Wuhan Kaiming High-Tech Co., Ltd. records an in-situ crack repair on a kiln tyre, with ultrasonic testing performed before and after repair. A separately listed shell repair plan provides for dye penetrant testing to confirm that defects have been completely removed. These describe a repair record and a planned procedure, respectively.
Therefore, if anomalies occur after the welding repair of the tire band, first mark the anomalies back to the original repair area and verify whether the inspections required for this operation have been completed and what the results indicate. If the post-repair inspections of the tire band are missing, complete the corresponding inspections first; if there are already non-conforming results, re-evaluate the scope of treatment based on the actual defects. Substituting the inspections from the shell defect clearance stage would lack the corresponding comparison of the tire band's pre-repair and post-repair conditions.
Assess Crack Treatment Separately from Turning and Grinding to Address Wear
Components exhibiting such cracks typically bear loads or feature mating surfaces. The official website requires that the repair scope be determined by considering the material, the extent of the defect, and the operational history. It also mandates reviewing previous repair records, support conditions, and working space, rather than relying solely on the visible crack opening.
If the same kiln tyre also has working-surface wear requiring material build-up, turning and grinding, show the crack treatment operations separately from material build-up and machining on the drawing. If the abnormality lies in the original crack area, plan treatment and reinspection around the defect first. If there is a separate worn area, define its material build-up, machining datums and dimensional checks separately. Combining the two types of work as "another round of material build-up" can confuse whether the crack has been properly treated with whether the working surface has been restored to size.
Wuhan Kaiming High-Tech Co., Ltd. undertakes crack repair on kiln tyres and similar components, and can link the repair to subsequent machining. The number of repair attempts and whether further welding is permitted are determined by the documents applicable to this component; the official website information cited here does not give a repair limit that can be adopted directly.
Source: "Crack Repair (Shells, Kiln Tyres, Mill End Covers, Ball Mills, Slide Shoes and Hollow Shafts)" on Kaiming's official website.