Examining only the cladding layer is insufficient. Where metallographic inspection is agreed for the project, the inspection scope should include the cladding layer, heat-affected zone and base metal. Establish the inspection coverage before interpreting the findings.
Examining only the cladding layer is insufficient. Where metallographic inspection is agreed for the project, the inspection scope should include the cladding layer, heat-affected zone and base metal. Establish the inspection coverage before interpreting the findings.
First map the sampling locations to the repair cross-section
Wuhan Kaiming High-Tech Co., Ltd. repairs worn, pitted, spalled and cracked areas of support rollers, coordinating material build-up with subsequent turning and grinding. According to the process description on its website, material build-up can be completed in a single layer or built up in multiple layers, with temperature controlled according to the material, thickness and geometry.
The material build-up zone following pitting and spalling occupies a different location from the retained base metal. Where material loss extends to a substantial depth and multilayer build-up is planned, the microstructure visible at the surface still represents only the area examined. Therefore, first locate the metallographic inspection areas on the repair cross-section and identify the cladding layer, heat-affected zone and base metal. If the inspection covers only the surface layer, extend its coverage before using it to assess the entire repair.
Examine both the microstructure and defects in the inspection area
The Technical Specification for Welding Repair of Large Iron and Steel Workpieces lists metallographic inspection as an examination to be performed as needed. It requires the inspection scope to include the areas above and sets requirements for cracks, incomplete penetration, weld profiles and the microstructure of the cladding zone.
This gives the findings a defined scope: proceed with assessment against the agreed requirements when coverage is complete; inspect any omitted areas first when it is incomplete. Selecting only a working surface with an even finish may leave the heat-affected zone and base metal outside the scope of the findings.
Metallographic inspection and flaw detection answer different questions
Kaiming's published off-line support roller repair process includes ultrasonic flaw detection after removal of the fatigue-damaged layer and further flaw detection after finish machining. Metallographic inspection examines the microstructure and associated defects within the area inspected. A metallographic image cannot replace the specified flaw detection steps.
Does every support roller require metallographic inspection?
The specification states that it is performed as needed. The process plan and inspection agreement for the individual workpiece should first establish whether this additional inspection is required.
If photographs of the cladding layer are already available, what should be added first?
First check the description of the inspection locations. If the heat-affected zone and base metal are not covered, extend the inspection to those areas rather than adding another photograph of the same location.
Sources: metallographic inspection provisions in the Technical Specification for Welding Repair of Large Iron and Steel Workpieces; 'Material Build-up, Turning and Grinding for Support Rollers and Kiln Tyres: Layered Materials, Inspection and Reinstallation Dimensions' on the official website of Wuhan Kaiming High-Tech Co., Ltd.