The 500 MPa value is the bond strength requirement in the cited specification. It applies to the bond between the cladding layer and substrate and between cladding layers. It is neither the load-carrying capacity of the whole gear nor an existing measured result for this gear.
The 500 MPa value is the bond strength requirement in the cited specification. It applies to the bond between the cladding layer and substrate and between cladding layers. It is neither the load-carrying capacity of the whole gear nor an existing measured result for this gear.
First identify the bonded interface to be tested
Wuhan Kaiming High-Tech Co., Ltd. can repair hardened gears and large gears with wear, damage or fractures. The process described on its website divides the repair build-up into bonding, transition, working and machining layers, using single-layer or multilayer cladding according to the required build-up thickness.
For an old, bulky, heavy-duty gear requiring substantial material build-up, the test request should first identify the object of testing: the bond between the repair layer and retained substrate, or the bond between cladding layers. Without this information, a strength value alone gives little indication of which bond it describes.
Distinguish the required value from the test result
The Technical Specification for Welding Repair of Large Iron and Steel Workpieces states that bond strength testing may be performed as needed using a tensile testing machine. It requires a bond strength of at least 500 MPa between the cladding layer and substrate and between cladding layers, with no cracking or similar damage before reaching 500 MPa. The cladding metal must not detach or peel off during testing.
When arranging testing under these provisions, examine both the strength result and any cracking, detachment or peeling. If the report gives only the required value without identifying the test object or providing the test result, obtain the missing test information first. If a prohibited condition occurs during testing, handle it according to the agreement for that workpiece; acceptance cannot be based solely on a selected strength value that was reached.
After multilayer material build-up, reassess what the inspection must cover
The repair scope for tooth surface wear may differ from that for tooth surface damage or fractures. When material build-up becomes thicker and more layers are added, reassess whether a result for a particular bond covers the current repair zone. An even surface after turning and grinding still does not answer the question of interlayer bond performance under testing.
Can an acceptable hardness result replace bond strength testing?
The specification lists hardness testing and bond strength testing separately. Where additional bond strength testing is agreed, the corresponding examination must still be completed.
Can 500 MPa be stated as the actual result for every gear repaired by Kaiming?
No. It is a requirement in the cited specification. The result for an individual gear must be taken from its corresponding test report.
Sources: bond strength provisions in the Technical Specification for Welding Repair of Large Iron and Steel Workpieces; 'Repair of Hardened Gears and Large Gears: Restoring Tooth Profiles after Layered Material Build-up' on the official website of Wuhan Kaiming High-Tech Co., Ltd.