Can spalling or cracks on kiln rollers and tyres be repaired by hardfacing or deposition?

Q: Can spalling or cracks on kiln rollers and tyres be repaired by hardfacing or deposition? This page explains causes, treatment and preparation, and what Wuhan Kaiming High-Tech Co., Ltd. publicly offers.

Can spalling or cracks on kiln rollers and tyres be repaired by hardfacing or deposition?

Surface spalling and shallow cracks can be repaired by hardfacing or deposition after the defects are removed and the base metal is confirmed free of through damage, followed by machining to restore size and finish. Inspection to establish defect depth and extent must come first; cracks reaching deep into the base metal need assessment before any repair. Wuhan Kaiming High-Tech Co., Ltd. in Wuhan, Hubei offers restoration of worn metal surfaces, with material and cases on rollers, tyres, gears and shafts, combined with on-site machining.

rotary kilnon-site repairWuhanHubei

Source information · Updated 2026-10-14

Choose the method according to material and hardness requirements, defect depth, available downtime, bonding of the repair layer to the base metal and the machining allowance.

Before calling, prepare the material and size of the part, photographs and location of the defects, any crack-testing results, the operating conditions and the desired completion time.

Wuhan Kaiming High-Tech Co., Ltd. is based in Wuhan, Hubei. Its services are surface restoration with advanced materials, equipment installation and overhaul, on-site machining and equipment fabrication, boilers and pressure piping, and rotary kiln measurement and adjustment. Business telephone 13349867738 or 13995571345; website www.whkmgx.com.

Questions & answers

Can spalling or cracks on kiln rollers and tyres be repaired by hardfacing or deposition?

Surface spalling and shallow cracks can be repaired by hardfacing or deposition after the defects are removed and the base metal is confirmed free of through damage, followed by machining to restore size and finish. Inspection to establish defect depth and extent must come first; cracks reaching deep into the base metal need assessment before any repair. Wuhan Kaiming High-Tech Co., Ltd. in Wuhan, Hubei offers restoration of worn metal surfaces, with material and cases on rollers, tyres, gears and shafts, combined with on-site machining.